Material: 95 WNiFe
Surface: Polished
Composition: 95% Tungsten, Nickel, Iron
Density: 18 gm/cc
Mil-Spec: T-21014 D, Class 3
Spec: ASTM -B777, Grade 3, Type II & III
Rockwell Hardness, HRC: 27 (34 Max)
Ultimate Tensile Strength, PSI, min.: 105,000
Yield Strength, 0.2% Offset, PSI, min.: 75,000
Elongation, % in 1": >3
Magnetic Property: Slightly Magnetic

Material: 99.95% Tungsten
Surface: Polished
Composition: 99.95% Tungsten
Density: 19.5 gm/cc

Material: W70Cu30
Surface: Polished
Composition: 70% Tungsten, 30% Copper
Density: 14.5 gm/cc

Material: 95WNiFe
Surface: Polished
Composition: 95% Tungsten, Nickel, Iron
Density: 18 gm/cc
Mil-Spec: T-21014 D, Class 3
Spec: ASTM -B777, Grade 3, Type II & III
Rockwell Hardness, HRC: 27 (34 Max)
Ultimate Tensile Strength, PSI, min.: 105,000
Yield Strength, 0.2% Offset, PSI, min.: 75,000
Elongation, % in 1": >3
Magnetic Property: Slightly Magnetic

Material: Tungsten Carbide
Surface: Polished
Grade: YG6, YG8, YG10
Density: 14.3 gm/cc

Material: 90 WNiFe
Surface: Polished
Composition: 90% Tungsten, 7% Nickel, 3% Iron
Density: 17 gm/cc
Magnetic Property: Slightly Magnetic

Material: 99.95% Tungsten
Surface: Polished
Diameters: 0.10 mm - 5mm
We use cookies to analyze website traffic and optimize your website experience. By accepting our use of cookies, your data will be aggregated with all other user data.